检索范围:
排序: 展示方式:
Creep-fatigue crack growth behavior in GH4169 superalloy
Dianyin HU, Xiyuan WANG, Jianxing MAO, Rongqiao WANG
《机械工程前沿(英文)》 2019年 第14卷 第3期 页码 369-376 doi: 10.1007/s11465-018-0489-7
关键词: crack growth rate creep-fatigue GH4169 superalloy CT specimen dwell time
CAO Jie, LUO Shimin, LIANG Lijian, LAI Jiaming, CHEN Shanming
《医学前沿(英文)》 2007年 第1卷 第3期 页码 287-293 doi: 10.1007/s11684-007-0055-x
Zhihua ZHANG,Huichen YU,Chengli DONG
《机械工程前沿(英文)》 2015年 第10卷 第4期 页码 418-423 doi: 10.1007/s11465-015-0362-x
Low cycle fatigue tests were conducted on the single crystal nickel-based superalloy, DD6, with different crystallographic orientations (i.e., [001], [011], and [111]) and strain dwell types (i.e., tensile, compressive, and balanced types) at a certain high temperature. Given the material anisotropy and mean stress, both orientation factor and stress range were introduced to the Smith, Watson, and Topper (SWT) stress model to predict the fatigue life. Experimental results indicated that the fatigue properties of DD6 depend on both crystallographic orientation and loading types. The fatigue life of the tensile, compressive, and balanced strain dwell tests are shorter than those of continuous cycling tests without strain dwell because of the important creep effect. The predicted results of the proposed modified SWT stress method agree well with the experimental data.
关键词: life prediction single crystal superalloy low cycle fatigue (LCF) crystallographic orientation strain dwell
Grindability of high-temperature alloy with ceramic alumina wheels
ZHANG Hongxia, CHEN Wuyi, CHEN Zhitong
《机械工程前沿(英文)》 2008年 第3卷 第2期 页码 139-145 doi: 10.1007/s11465-008-0040-3
关键词: metallographic topography grinding GH2132 resistance decrease
Novel casting processes for single-crystal turbine blades of superalloys
Dexin MA
《机械工程前沿(英文)》 2018年 第13卷 第1期 页码 3-16 doi: 10.1007/s11465-018-0475-0
This paper presents a brief review of the current casting techniques for single-crystal (SC) blades, as well as an analysis of the solidification process in complex turbine blades. A series of novel casting methods based on the Bridgman process were presented to illustrate the development in the production of SC blades from superalloys. The grain continuator and the heat conductor techniques were developed to remove geometry-related grain defects. In these techniques, the heat barrier that hinders lateral SC growth from the blade airfoil into the extremities of the platform is minimized. The parallel heating and cooling system was developed to achieve symmetric thermal conditions for SC solidification in blade clusters, thus considerably decreasing the negative shadow effect and its related defects in the current Bridgman process. The dipping and heaving technique, in which thin-shell molds are utilized, was developed to enable the establishment of a high temperature gradient for SC growth and the freckle-free solidification of superalloy castings. Moreover, by applying the targeted cooling and heating technique, a novel concept for the three-dimensional and precise control of SC growth, a proper thermal arrangement may be dynamically established for the microscopic control of SC growth in the critical areas of large industrial gas turbine blades.
关键词: superalloy investment casting Bridgman process directional solidification single crystal turbine blade
胡壮麒,孙文儒,宋洪伟
《中国工程科学》 2005年 第7卷 第3期 页码 17-26
阐述了磷、硼的微合金强化作用。磷、硼微合金强化可成倍提高变形合金的持久寿命、降低蠕变速率一个数量级以上。利用磷、硼微合金化技术可发展长寿命高温合金,提高IN718合金的使用温度发展可在700℃长期使用并具有优良性能的涡轮盘合金。
王海舟,李美玲,庄景云
《中国工程科学》 2011年 第13卷 第10期 页码 19-27
采用原位统计分布分析表征技术系统研究了GH169高温合金压气机盘纵断面不同部位铌分布的规律。
激光修复Inconel 718镍基高温合金过程中Laves相的原位调控新方法 Article
隋尚, 李浩胜, 李祚, 赵轩, 马良, 陈静
《工程(英文)》 2022年 第16卷 第9期 页码 239-246 doi: 10.1016/j.eng.2021.08.030
激光修复Inconel 718 高温合金通常由组织差异明显的基材区锻造组织和激光修复区熔覆组织两部分构成。其中,激光熔覆区内Laves 相的尺寸、形貌和分布对激光修复Inconel 718 高温合金的力学性能有重要影响。然而,考虑高温条件下基材区组织与性能的劣化,激光熔覆区内的Laves 相难以通过后热处理进行优化。基于此,本文提出了一种原位激光热处理(in situ laser heat-treatment, ISLHT)工艺,该方法可以通过激光加热先前的沉积层,在不影响基材区的基础上,基于优化的工艺参数,有效调控激光熔覆区内Laves 相的尺寸和形貌。本文采用热电偶和红外摄像机来监测和分析ISLHT过程中的热循环和实时温度分布,并通过光学显微镜、扫描电子显微镜、电子探针等观察分析微观组织结构和元素偏析。研究发现,ISLHT 工艺可以有效地改变Laves 相的形态和尺寸,使Laves 相从连续的大尺寸长条状转变为离散的细小颗粒状。其中,有效温度范围和持续时间是影响ISLHT过程中Laves 相演变的两个主要因素。有效温
度范围由激光线能量密度决定,峰值温度随线能量密度的增加而增加。此外,可以通过同时增加激光功率和扫描速度来降低温度幅度。最后,提出了基于ISLHT 工艺进行Laves 相调控的流程图,并实现了具有细小颗粒Laves相的单壁墙试样的沉积。
关键词: 激光修复 原位激光热处理 Inconel 718合金 Laves相
基于自组织映射的增材制造中数据驱动式微观组织和显微硬度设计 Article
甘政涛, 李恒阳, Sarah J. Wolff, Jennifer L. Bennett, Gregory Hyatt, Gregory J. Wagner, 曹简, Wing Kam Liu
《工程(英文)》 2019年 第5卷 第4期 页码 730-735 doi: 10.1016/j.eng.2019.03.014
为了在镍基高温合金的增材制造(AM)中设计微观组织和显微硬度,本研究提出了一种新的数据驱动方法,该方法结合了物理模型、实验测量和数据挖掘方法。该模拟基于计算热流体动力学(CtFD)模型,可以获得热行为、凝固参数(如冷却速度)和凝固层的稀释率。根据计算出的热信息, 可利用经过充分测试的力学模型估算枝晶臂间距和显微硬度。通过实验测定试样的微观结构和显微硬度,与模拟值进行比较验证。为了实现过程-组织-性能(PSP)关系的可视化,模拟及实验数据集被输入到数据挖掘模型——自组织映射(SOM)中。在多目标下,工艺参数的设计窗口可以从可视化映射中得到。这种被提出的方法可用于AM和其他数据密集型工艺过程。过程、组织和性能之间的数据驱动联系可能会有利于在线过程监控控制,从而获得理想的微观组织和力学性能。
标题 作者 时间 类型 操作
Creep-fatigue crack growth behavior in GH4169 superalloy
Dianyin HU, Xiyuan WANG, Jianxing MAO, Rongqiao WANG
期刊论文
Effects of parenteral nutrition with and without GH on the GH/IGF-1 axis after hepatectomy in hepatocellular
CAO Jie, LUO Shimin, LIANG Lijian, LAI Jiaming, CHEN Shanming
期刊论文
LCF behavior and life prediction method of a single crystal nickel-based superalloy at high temperature
Zhihua ZHANG,Huichen YU,Chengli DONG
期刊论文
Grindability of high-temperature alloy with ceramic alumina wheels
ZHANG Hongxia, CHEN Wuyi, CHEN Zhitong
期刊论文